Hostname: page-component-7bb8b95d7b-lvwk9 Total loading time: 0 Render date: 2024-09-17T12:50:18.270Z Has data issue: false hasContentIssue false

X-ray Fractographic Study on TiAl Alloys with Various Types of Microstructures

Published online by Cambridge University Press:  06 March 2019

Hiroyuki Tabata
Affiliation:
Industrial Research Institute of Islrikawa Ro-1 Tomizii, Kanazawa 920-02, Japan
Zenjiro Yajima
Affiliation:
Department of Engineering Science Kanazawa institute of Technology 7-1 Oogigaoka, Nonoichi, Kanazawa 921, Japan
Yukio Hirose
Affiliation:
Department of Materials Science and Engineering Kanazawa University Kakuma, Kanazawa 920-11, Japan
Get access

Abstract

The fracture toughness test was conducted on γ + α2 two-phase TiAl alloys with lamellar, duplex and near-y structures. The x-ray fractographic technique was applied to the fracture, surfaces. The plastic zone size my was determined on the basis of the distributions of the residual stress and the half-value breadth beneath the fracture surfaces. Although the fracture mode shows microstructure dependence, ωγ is related to the fracture toughness value KIC and the yield stress σY as:

ωy=α(KIC/σY)

where α is 0.13.

Type
V. Residual Stress, Crystallite Size and rms Strain Determination by Diffraction Methods
Copyright
Copyright © International Centre for Diffraction Data 1994

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

1. Tuyama, S., Mitau, S., and Minakawa, K., “Effect of aluminum content and microstructure on fracture toughness of binary TiAl alloys,” in: “Microstructure/Property Relationships in Titanium Aluminides and Alloys“; Kim, Y-W. and Boyer, R. R., ed., TMS, Warrendale, 213 (1991).Google Scholar
2. Chan, K. S. and Kim, Y-W., “Influence of micro structure on crack-tip micromechanics and fracture behaviors of two-phase TiAl alloy,” Me tall. Trans., 23A: 1663 (1992).Google Scholar
3. Chan, K. S., “Toughening mechanisms in titanium aluminides”, Metall. Trans., 24A: 569 (1993).Google Scholar
4. Huang, S. C. and Hail, E. L., “Plastic deformation and fracture of binarv TiAl-base alloys”, Metall. Trans., 22A: 427 (1991).Google Scholar
5. Tabata, H., Yajima, Z., Sasaki, T. and Hirose, Y., “Application of X-ray examination to fracture surface of TiAl intermetallic compound”, To be published in “ Vol, 37 of Advances in X-Ray Analysis”, (1994).Google Scholar
6. Tabata, H., Sasaki, T., Yajima, Z., and Hirose, Y., “X-ray measurement of elastic deformation in titanium aluminide alloys,” Proceedings of The 30th Symposium on X-Ray Studies on Mechanical Behavior of Materials, Soc. Mat. Sci., Japan, Kyoto, 141 (1994).Google Scholar
7. ASTM Standard, “Standard Test Method for Plane-Strain Fracture Toughness of Metallic Materials,” Part 10, E 399-81 (1931).Google Scholar