Sol-gel synthesis of textured lanthanum titanate thin films

Published online by Cambridge University Press:  31 January 2011

Mary M. Sandstrom
Affiliation:
Department of Materials and Metallurgical Engineering, New Mexico Institute of Mining and Technology, Socorro, New Mexico 87801
Paul Fuierer
Affiliation:
Department of Materials and Metallurgical Engineering, New Mexico Institute of Mining and Technology, Socorro, New Mexico 87801
Get access

Abstract

Control over crystallographic orientation in thin films is important, particularly with highly anisotropic structures. Because of its ferroelectric nature, the layered perovskite La2Ti2O7 has interesting piezoelectric and electrooptic properties that may be exploited when films are highly textured. Sol-gel films with an orientation factor of greater than 95% were fabricated without relying on epitaxial (lattice-matching) growth from the substrate. Film orientation and crystallization were confirmed by x-ray diffraction, scanning electron microscopy, atomic force microscopy, and optical measurements. The particle sizes in all precursor solutions were measured by dynamic light scattering experiments. Experimental results indicate that film orientation is a function of precursor solution concentration, size of the molecular clusters in the solution, and film thickness.

Type
Articles
Copyright
Copyright © Materials Research Society 2003

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

Nanamatsu, S., Kimura, M., Doi, K., Matsushita, S., and Yamada, N., Ferroelectrics 8, 511 (1974).CrossRefGoogle Scholar
Kimura, M., Nanamatsu, S., Doi, K., Matsushita, S., and Takahashi, M., Jpn. J. Appl. Phys. 11, 904 (1972).CrossRefGoogle Scholar
Fuierer, P.A. and Newnham, R.E., J. Am. Ceram. Soc. 74, 2876 (1991).CrossRefGoogle Scholar
Ishizawa, N., Marumo, F., Iwai, S., Kimura, M., and Kawamura, T., Acta. Crystallogr. B 36, 763 (1980).CrossRefGoogle Scholar
Ishizawa, N., Marumo, F., Iwai, S., Kimura, M., and Kawamura, T., Acta. Crystallogr. B 38, 368 (1982).CrossRefGoogle Scholar
Gasperin, M., Acta. Crystallogr. B 31, 2129 (1975).CrossRefGoogle Scholar
Prasadarao, A.V., Selvaraj, U., Komarneni, S., and Bhalla, A.S., Ferroelectric Lett. 14(3–4), 65 (1992).CrossRefGoogle Scholar
Jeon, S.J., Cho, K.H., Nam, H.D., Park, C.W., Jang, S.W., and Lee, H.Y., J. Kor. Phys. Soc. 32, (Suppl. issue) S1657 (1998)Google Scholar
Dickerson, B.D., Masaya, N., Song, Y.J., Nam, H.D., and Desu, S.B., in Ferroelectric Thin Films IV, edited by Desu, S.B., Tuttle, B.A., Ramesh, R., and Shiosaki, T. (Mater. Res. Soc. Symp. Proc. 361, Pittsburgh, PA 1995), pp. 197202.Google Scholar
Seo, J.W., Fompeyrine, J., and Locquet, J.P., in Superconducting and Related Oxides: Physics and Nanoengineering III, Proceedings of the SPIE, edited by Pavuna, D., Bozovic, I. (SPIE-Int. Soc. Opt. Eng, Billingham, WA, 1998), Vol. 3481, pp. 326333CrossRefGoogle Scholar
Pecora, R., Dynamic Light Scattering: Applications of Photon Correlation Spectroscopy (Plenum Press, New York, 1985).CrossRefGoogle Scholar
Fuierer, P.A., Li, B., and Jeon, H.S., J. Sol-Gel Sci. Technol. (2003, in press).Google Scholar
Lotgering, F.K., J. Inorg. Nucl. Chem. 9, 113 (1959).CrossRefGoogle Scholar
Mullins, W.W., Metal Surfaces (American Society for Metals, Metals Park, OH, 1963).Google Scholar
Meiksin, Z.H., Thin and Thick Films for Hybrid Microelectronics (Lexington Books, Lexington, MA, 1976).Google Scholar
Cheng, J.G., Meng, X.J., Tang, J., Guo, S.L., Chu, J.H., Wang, M., Wang, H., and Wang, Z.J., Amer. Ceram. Soc. 83, 22616 (2000).CrossRefGoogle Scholar
Shwartz, R.W., Clem, P.G., Voigt, J.A., Byhoff, E.R., Stry, M. Van, Headly, T.J., and Missert, N.A., J. Am. Ceram. Soc. 82, 2359 (1999).CrossRefGoogle Scholar
Hoffman, U., Hasenkox, U., Waser, P., Jia, J.L., and Urban, K., in Epitaxial Oxide Thin Films III, edited by Schlom, D.G., Eom, C-B., Hawley, M.E., Foster, C.M., and Speck, J.S. (Mater. Res. Soc. Symp. Proc. 474, Pittsburgh, PA, 1997), pp. 914.Google Scholar
Fuierer, P.A. and Li, B., J. Am. Ceram. Soc. 85, 299 (2002).CrossRefGoogle Scholar
Brinker, C.J. and Scherer, G.W., Sol-Gel Science: the Physics and Chemistry of Sol-Gel Processing (Academic Press, Boston, MA, 1990)Google Scholar
Chen, C., Ryder, D.F., Jr., and Spurgeon, W.A.J., Amer. Ceram. Soc. 72, 1495 (1989).CrossRefGoogle Scholar