Investigation of Ni3Al-matrix composites strengthened by TiC

Published online by Cambridge University Press:  03 March 2011

Bingchu Mei
Affiliation:
National Lab of Advanced Technology for Composites, Wuhan University of Technology, Wuhan 430070, People's Republic of China
Runzhang Yuan
Affiliation:
National Lab of Advanced Technology for Composites, Wuhan University of Technology, Wuhan 430070, People's Republic of China
Xinlong Duan
Affiliation:
National Lab of Advanced Technology for Composites, Wuhan University of Technology, Wuhan 430070, People's Republic of China
Get access

Abstract

In this paper, the possibilities of preparing TiC-reinforced Ni3Al-matrix composites by SM (self-propagating high temperature synthesis and melting process) were examined. Two kinds of composites, namely, commercial TiC-reinforcement and synthesized TiC-reinforcement Ni3Al-matrix composites, were fabricated. The effects of particle size of the commercial TiC on the mechanical properties of the Ni3Al-matrix composites were studied. The results show that the mechanical properties of the composites decrease with increasing particle size of the commercial TiC. The microstructures of 35 wt. % TiC + 65 wt. % Ni3Al composites produced by SM technology from the four elements Ti, C, Ni, and Al were examined. The results show that in these composites, the particle size of TiC synthesized in situ is fine and that the materials have considerable high-temperature bending strength and fracture toughness.

Type
Articles
Copyright
Copyright © Materials Research Society 1993

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

1Liu, C. T. and Stiegler, J. O., Mater. Eng. 100 (5), 29 (1984).Google Scholar
2Stoloff, N. S., in High-Temperature Ordered Intermetallic Alloys, edited by Koch, C. C., Liu, C. T., and Stoloff, N. S. (Mater. Res. Soc. Symp. Proc. 39, Pittsburgh, PA, 1985), p. 3.Google Scholar
3Schwetz, K. A., Grellner, W., and Lpp, A., in “Proc. 2nd Int. Conf. on the Science of Hard Materials,” edited by Almond, E. A., Brookes, C. A., and Harren, R., Rhodes, September 23–28, 1984, in Inst. Phys. Conf. Ser. 75, 413 (1986).Google Scholar
4Weihs, T. P., Zinoviev, V., Viens, D. V., and Schulson, E. M., Acta Metall. 34, 1395 (1986).Google Scholar
5Schulson, E. M., Weihs, T. P., Viens, D. V., and Baker, J., Acta Metall. 23, 1287 (1985).Google Scholar
6Cottrell, A. H., Dislocations and Plastic Flow in Crystals (Clarendon, Oxford, 1953), p. 99.Google Scholar
7Perry, R. H., Chemical Engineers' Handbook, 4th ed. (McGraw-Hill Book Company, New York, 1963).Google Scholar
8Gray, D. E., American Institute of Physics Handbook, 3rd ed. (McGraw-Hill Book Company, New York, 1972).Google Scholar
9Trinklepaugh, J. R. and Gradall, W. B., Cermets (Reinhold Publishing Corp., 1960), p. 11.Google Scholar