No CrossRef data available.
Article contents
Metallurgical quality characterization of nickel-basedsuperalloys
Published online by Cambridge University Press: 22 May 2007
Abstract
A new image analyzer, Thixomet®, has been developed with the ability to create “panoramic” images of material microstructure for investigations. Capabilities of the Thixomet image analyzer for material microstructural characterization are demonstrated with examples of nickel-based superalloys. Practical use of the Thixomet for controlling material properties by characterizing their microstructure is demonstrated.
- Type
- Research Article
- Information
- Metallurgical Research & Technology , Volume 104 , Issue 5: Haut-fourneauGalvanisationUtilisation de l'acier , May 2007 , pp. 258 - 262
- Copyright
- © La Revue de Métallurgie, 2007