Surface analysis of the selective oxidation during austeniticannealing of CMnSi high strength steel

Published online by Cambridge University Press:  10 April 2009

Get access

Abstract

The selective oxidation of three CMnSi steels with different C levels was studied by XPS. The formation of a gradually covering SiO2 film is observed until a transition temperature above which the oxide film disappears, resulting in a renewed appearance of metallic iron at the surface. This change in oxidation behavior is thought to be due to the SiO2 reduction by solute C which is thermodynamically favorable at high temperature. At the same time the precipitation of a BN film on the metallic surface was observed which prevented any further oxidation.

Type
Research Article
Copyright
© La Revue de Métallurgie, 2009

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)