Behaviour of a CoCrMo Implant Alloys in Ringer??s Type Solutions Studied by Electrochemical and Surface Analysis Techniques

Published online by Cambridge University Press:  05 August 2007

J Mirza Rosca
Affiliation:
University of Las Palmas de Gran Canaria,Spain
A Santana Lopez
Affiliation:
University of Las Palmas de Gran Canaria,Spain
D Mareci
Affiliation:
Technical University Iasi,Romania
Get access

Extract

Extended abstract of a paper presented at Microscopy and Microanalysis 2007 in Ft. Lauderdale, Florida, USA, August 5 – August 9, 2007