Hostname: page-component-5c6d5d7d68-thh2z Total loading time: 0 Render date: 2024-08-16T13:12:15.536Z Has data issue: false hasContentIssue false

Cross-Sectional Sample Preparation and Analysis of Intergranular Stress Corrosion Cracks in FE-NI-CR Alloys.

Published online by Cambridge University Press:  02 July 2020

L.E. Thomas
Affiliation:
Mechanical and Materials Engineering, Washington State University, Pullman, WA99352
S.M. Bruemmer
Affiliation:
Pacific Northwest National Laboratory, Richland, WA99353
Get access

Extract

Transmission electron microscopy in its modern high-resolution analytical form has great potential for elucidating mechanisms of environmental cracking in structural alloys and other materials. Apart from a few pioneering efforts, the difficulties of preparing suitable samples with the original corrosion structures preserved in narrow crack tips have limited contributions of TEM in this area. Recent work involving cross-sectional crack preparation has focused on intergranular stress-corrosion cracking of Fe- and Ni-base stainless alloys in high-temperature water. This presentation will illustrate preparation methods that have proven successful, and describe limitations of the analysis.

The method for preparing cross-section samples suitable for high-resolution TEM characterization is based on earlier work by Lewis et al. It involves preparing a thin section containing cracks filled with epoxy, dimple grinding selected locations near the crack tip, and ion milling. Figure 1 schematically illustrates this method. The first step is to preserve the crack opening characteristics present under loading and protect the crack surfaces during thinning.

Type
Precision Specimen Preparation
Copyright
Copyright © Microscopy Society of America

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

1.Scamans, G.M. and Swann, P.R., Corrosion Sci. 18 (1978) 983.CrossRefGoogle Scholar
2.Newcombe, S.B., Boothroyd, C.B., and Stobbs, W.M., J. Micros., 140 (1985) 195.CrossRefGoogle Scholar
3.Nisbet, W.J., Lorimer, G.W., and Newman, R.C., Corrosion Sci. 35 (1993) 457.CrossRefGoogle Scholar
4.Lewis, N., Perry, D.J., and Bunch, M.L., Proc. Ann MSA Meeting (1995) 550.CrossRefGoogle Scholar