Hostname: page-component-788cddb947-rnj55 Total loading time: 0 Render date: 2024-10-18T22:51:48.263Z Has data issue: false hasContentIssue false

Nanoindentation in Tin/Nbn Multilayers and Thin Films Examined Using Transmission Electron Microscopy

Published online by Cambridge University Press:  02 July 2020

S.J. Lloyd
Affiliation:
Department of Materials Science and Metallurgy, University of Cambridge, Cambridge, CB2 3QZ, UK
J.E. Pitchford
Affiliation:
Department of Materials Science and Metallurgy, University of Cambridge, Cambridge, CB2 3QZ, UK
J.M. Molina-Aldareguia
Affiliation:
Department of Materials Science and Metallurgy, University of Cambridge, Cambridge, CB2 3QZ, UK
Z.H. Barber
Affiliation:
Department of Materials Science and Metallurgy, University of Cambridge, Cambridge, CB2 3QZ, UK
M.G. Blamire
Affiliation:
Department of Materials Science and Metallurgy, University of Cambridge, Cambridge, CB2 3QZ, UK
W.J. Clegg
Affiliation:
Department of Materials Science and Metallurgy, University of Cambridge, Cambridge, CB2 3QZ, UK
Get access

Extract

Nanoindentation allows the hardness of thin coatings and synthetic multilayer structures to be measured, since indentation depths can be as little as a few 10s of nm. In combination with the cross-sectional transmission electron microscopy (TEM) analysis described here it is possible to observe the deformation structure under an indent, and potentially to understand deformation mechanisms on a nm scale in a wide variety of materials. Synthetic multilayers are a particularly interesting system to investigate. Variations in hardness with the multilayer compositional repeat distance (A) have been reported for several systems. The highest hardnesses, which are in excess of what a simple “rule of mixtures” would predict, occur in nitride multilayers at A ∼5nm. Here we present some preliminary results showing the deformation structure in both a monolithic NbN film and a TiN/NbN multilayer in which both components have the rQck salt structure with lattice parameters 0.424nm (TiN) and 0.439nm (NbN).

Type
Future of Microscopy: Ceramics, Composites, and Cement
Copyright
Copyright © Microscopy Society of America

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

1.Barnett, S.A. and Shinn, M., Annu. Rev. Mater. Sci 24 (1994) 481.CrossRefGoogle Scholar
2.Barber, Z.H.et al., IEEE Trans. Appl. Supercond. 3 (1993) 2054.CrossRefGoogle Scholar
3.Ishitani, T.et al., J. Electron Microsc. 43 (1994) 322.Google Scholar
4.Shinn, M.et al., J. Mater. Res. 7 (1992) 901.CrossRefGoogle Scholar
5. The authors are grateful to the EPSRC, Trinity Hall, Cambridge (SJL), NEDO, Japan (JEP) and the Basque Government (JMM-A) for financial support.Google Scholar