Correlative Micro-Compression and 3D X-ray Nanotomography Study of the Fracture Behavior of TCP Phases in an Additively Manufactured Ni-Base Superalloy

Published online by Cambridge University Press:  22 July 2022

Michael Sommerschuh*
Affiliation:
Institute of Micro- and Nanostructure Research (IMN) & Center for Nanoanalysis and Electron Microscopy (CENEM), Interdisciplinary Center for Nanostructured Films (IZNF), Department of Materials Science and Engineering, Friedrich-Alexander University Erlangen-Nürnberg (FAU), Erlangen, Bavaria, Germany
Janis Wirth
Affiliation:
Institute of Micro- and Nanostructure Research (IMN) & Center for Nanoanalysis and Electron Microscopy (CENEM), Interdisciplinary Center for Nanostructured Films (IZNF), Department of Materials Science and Engineering, Friedrich-Alexander University Erlangen-Nürnberg (FAU), Erlangen, Bavaria, Germany
Benoit Merle
Affiliation:
Materials Science & Engineering - Institute I, Interdisciplinary Center for Nanostructured Films (IZNF), Friedrich-Alexander-University Erlangen-Nürnberg (FAU), Erlangen, Bavaria, Germany
Julian Pistor
Affiliation:
Chair of Materials Science and Engineering for Metals (WTM), Friedrich-Alexander-University Erlangen-Nürnberg (FAU), Erlangen, Bavaria, Germany
Silvan Englisch
Affiliation:
Institute of Micro- and Nanostructure Research (IMN) & Center for Nanoanalysis and Electron Microscopy (CENEM), Interdisciplinary Center for Nanostructured Films (IZNF), Department of Materials Science and Engineering, Friedrich-Alexander University Erlangen-Nürnberg (FAU), Erlangen, Bavaria, Germany
Thomas Przybilla
Affiliation:
Institute of Micro- and Nanostructure Research (IMN) & Center for Nanoanalysis and Electron Microscopy (CENEM), Interdisciplinary Center for Nanostructured Films (IZNF), Department of Materials Science and Engineering, Friedrich-Alexander University Erlangen-Nürnberg (FAU), Erlangen, Bavaria, Germany
Carolin Körner
Affiliation:
Chair of Materials Science and Engineering for Metals (WTM), Friedrich-Alexander-University Erlangen-Nürnberg (FAU), Erlangen, Bavaria, Germany
Mathias Göken
Affiliation:
Materials Science & Engineering - Institute I, Interdisciplinary Center for Nanostructured Films (IZNF), Friedrich-Alexander-University Erlangen-Nürnberg (FAU), Erlangen, Bavaria, Germany
Benjamin Apeleo Zubiri
Affiliation:
Institute of Micro- and Nanostructure Research (IMN) & Center for Nanoanalysis and Electron Microscopy (CENEM), Interdisciplinary Center for Nanostructured Films (IZNF), Department of Materials Science and Engineering, Friedrich-Alexander University Erlangen-Nürnberg (FAU), Erlangen, Bavaria, Germany
Erdmann Spiecker*
Affiliation:
Institute of Micro- and Nanostructure Research (IMN) & Center for Nanoanalysis and Electron Microscopy (CENEM), Interdisciplinary Center for Nanostructured Films (IZNF), Department of Materials Science and Engineering, Friedrich-Alexander University Erlangen-Nürnberg (FAU), Erlangen, Bavaria, Germany

Abstract

Image of the first page of this content. For PDF version, please use the ‘Save PDF’ preceeding this image.'
Type
Advanced 3D Imaging and Analysis Methods for New Opportunities in Material Science
Copyright
Copyright © Microscopy Society of America 2022

References

Reed, RC in “The Superalloys: Fundamentals and Applications” (2006) p. 1.CrossRefGoogle Scholar
Wilson, AS, Materials Science and Technology 33(9) (2017), p. 1108.CrossRefGoogle Scholar
Geddes, B, León, H and Huang, XM in “Superalloys: Alloying and Performance” (2010).CrossRefGoogle Scholar
Cervellon, A et al. , Acta Materialia 188 (2020), p. 131.CrossRefGoogle Scholar
Hrutkay, K and Kaoumi, D, Materials Science and Engineering A 599 (2014), p. 196.CrossRefGoogle Scholar
Caron, P, Materials Science & Engineering A 254(1-2) (1998), p. 1.Google Scholar
Ramsperger, M, Singer, RF and Körner, C, Metallurgical and Materials Transactions A 47(3) (2016), p. 1469.CrossRefGoogle Scholar
Pistor, J and Körner, C, Materials Letters: X 1 (2019), p. 100003.Google Scholar
We gratefully acknowledge financial support by the German Research Foundation (DFG) within the frameworks of the research training group GRK1896 “In situ Microscopy with Electrons, X-rays and Scanning Probes”, the project SP648/8 “High-resolution X-ray microscopy for correlative tomography, high throughput screening and in situ mechanical testing of structural and functional materials” (project number 316992193) and the projects A6, A7 and B2 of the collaborative research center SFB Transregio/103 “From Atoms to Turbine Blades - a Scientific Approach for Developing the Next Generation of Single Crystal Superalloys” (project number 190389738).Google Scholar