Fractographic Evaluation of Medium Carbon Steels with Low Hot Ductility

Published online by Cambridge University Press:  01 August 2002

O. Dremailova
Affiliation:
Materials Technology Laboratory, CANMET, Ottawa, Ontario, K1A 0G1
D. Emadi
Affiliation:
Materials Technology Laboratory, CANMET, Ottawa, Ontario, K1A 0G1
E. Essadiqi
Affiliation:
Materials Technology Laboratory, CANMET, Ottawa, Ontario, K1A 0G1
J. R. Brown
Affiliation:
Materials Technology Laboratory, CANMET, Ottawa, Ontario, K1A 0G1

Abstract

Image of the first page of this content. For PDF version, please use the ‘Save PDF’ preceeding this image.'
Type
Abstract
Copyright
Copyright © Microscopy Society of America 2002