Hostname: page-component-788cddb947-xdx58 Total loading time: 0 Render date: 2024-10-15T03:23:48.186Z Has data issue: false hasContentIssue false

Mechanical Properties of Bond Coatings and Ni-based Superalloys at Extreme Temperatures

Published online by Cambridge University Press:  22 July 2022

Sanjit Bhowmick
Affiliation:
Bruker, Minneapolis, Minnesota, USA
Eric Hintsala
Affiliation:
Bruker, Minneapolis, Minnesota, USA

Abstract

Image of the first page of this content. For PDF version, please use the ‘Save PDF’ preceeding this image.'
Type
Mechanisms of High Strain Rate Plastic Deformation: Plasticity and Microstructural Evolutions of Adiabatic Shear Bands
Copyright
Copyright © Microscopy Society of America 2022

References

Jaya, B., Bhowmick, S., Asif, S., Jayaram, V., J. Mater. Res. 30 (2015) 3343.10.1557/jmr.2015.285CrossRefGoogle Scholar
Jaya, B., Bhowmick, S., Asif, S., Warren, O., Jayaram, V., Phil. Mag., 95 (2015) 1946.10.1080/14786435.2015.1010623CrossRefGoogle Scholar
Alam, M. D., Kamat, S. V., Jayaram, V. and Das, D. K., Acta Mat., 67 (2014) 278.10.1016/j.actamat.2013.12.033CrossRefGoogle Scholar
SB acknowledges collaboration support of Prof. Vikram Jayaram (Indian institute of science) and Prof. Nagamani Jaya Balila (Indian Institute of Bombay).Google Scholar