Model Materials for Irradiated Fuels: Study of Local Mechanical Behavior Using Nanoindentation and Microstructural Analysis

Published online by Cambridge University Press:  27 August 2014

Nathalie Payraudeau Le Roux
Affiliation:
INSA-Lyon, MATEIS CNRS UMR5510, F-69621 Villeurbanne, France
Sylvain Meille
Affiliation:
INSA-Lyon, MATEIS CNRS UMR5510, F-69621 Villeurbanne, France
Cyril Langlois
Affiliation:
INSA-Lyon, MATEIS CNRS UMR5510, F-69621 Villeurbanne, France
Isabelle Zacharie-Aubrun
Affiliation:
CEA, DEN, DEC Cadarache, 13108 St Paul Lez Durance, France
Thierry Douillard
Affiliation:
INSA-Lyon, MATEIS CNRS UMR5510, F-69621 Villeurbanne, France
Jean-Marie Gatt
Affiliation:
CEA, DEN, DEC Cadarache, 13108 St Paul Lez Durance, France

Abstract

Image of the first page of this content. For PDF version, please use the ‘Save PDF’ preceeding this image.'
Type
Abstract
Copyright
Copyright © Microscopy Society of America 2014 

References

[1] Anstis, G. R, et al. (1981), Journal of the American Ceramic Society, 64:533-538.Google Scholar
[2] Dukino, R. D, et al. (1992), Journal of the American Ceramic Society, 75: 3299-3304.Google Scholar