Study of Ionic Grain Boundary Segregation in Thermally Grown Alumina on Single-Crystal Superalloys
Published online by Cambridge University Press: 08 April 2017
Extract
Core share and HTML view are not available for this content. However, as you have access to this content, a full PDF is available via the ‘Save PDF’ action button.
Extended abstract of a paper presented at Microscopy and Microanalysis 2011 in Nashville, Tennessee, USA, August 7–August 11, 2011.