Conventional fusion welding procedures are not likely to be useful for joining NiAl because of its poor low temperature ductility. Thus, the potential use of this material could be limited. This study was designed to demonstrate the feasibility of using a diffusion brazing process to fabricate NiAl components. A unique feature of this process is the development of self-generated filler metal through elevated temperature vacuum exposure. Butt joints were made in extruded bar and joint quality was evaluated using metallographic techniques. Sound joints, which were produced with complete grain growth across the braze interface, were indistinguishable from the base metal. Thus, the feasibility of diffusion brazing NiAl was established.

Type
Research Article
Copyright
Copyright © Materials Research Society 1995

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

1. Darolia, R., JOM 43, 4449, March(1991).Google Scholar
2. Anton, D. L., Shah, D. M., Duhl, D. N., & Giamei, A.F., JOM 41, 1217, September (1989).Google Scholar
3. Pattee, H. E., High Temperature Brazing, Welding Research Council Bulletin No. 187, (1973).Google Scholar
4. Rechtein, J. J., et al. , J. Applied Physics 38, 8(1967).Google Scholar
5. Jacobi, H., and Stahl, R., J. Phys. Chem. Solids 34, 17371748, (1973). Pergamon Press.Google Scholar