Hostname: page-component-77c89778f8-m42fx Total loading time: 0 Render date: 2024-07-19T18:13:54.988Z Has data issue: false hasContentIssue false

High Glass Transition TemperatÜRe Electro-Optic Polymers

Published online by Cambridge University Press:  16 February 2011

Chengjiu Wu
Affiliation:
Alliedsignal Inc., Research And Technology, Morristown, Nj 07960
Karl Beeson
Affiliation:
Alliedsignal Inc., Research And Technology, Morristown, Nj 07960
Paul Ferm
Affiliation:
Alliedsignal Inc., Research And Technology, Morristown, Nj 07960
Charles Knapp
Affiliation:
Alliedsignal Inc., Research And Technology, Morristown, Nj 07960
Michael J. Mcfarland
Affiliation:
Alliedsignal Inc., Research And Technology, Morristown, Nj 07960
Ajay Nahata
Affiliation:
Alliedsignal Inc., Research And Technology, Morristown, Nj 07960
Jianhui Shan
Affiliation:
Alliedsignal Inc., Research And Technology, Morristown, Nj 07960
James T. Yardley
Affiliation:
Alliedsignal Inc., Research And Technology, Morristown, Nj 07960
Get access

Abstract

Disperse Red-1 type chromophores were attached to the backbones of PMMA, polyvinyl-phenol as well as the styrene-Maleimide alternative copolymer and glass transition temperatures of these three polymer derivatives were in the range of 125, 165, and 245°C, respectively. We have also, for the first time, attached EO chromophores to some thermostable cardo-polymers. Fluorene derivatives in which the 2- and 7-positions were substituted with an electron accepting and an electron donating substitutem, respectively, were made polymerizable through their reactive functional groups at the 9,9′-positions. Various condensation polymers were prepared. These polymers are amorphous, film-forming, thermostable, and having Tg ranging from 150 to 300°C. These polymers exhibit strong electro-optic properties after electrode poling. Thermal stabilities of these polymers were compared by following the spectral decay of the chromophore and the decay of the electro-optic coefficient. The loss of EO activity at elevated temperature can be realized as a combination of chromophore reorientation and chemical degradation.

Type
Research Article
Copyright
Copyright © Materials Research Society 1994

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

1. Singer, K.D., Sohn, J.E., King, L. A., Gordon, H.M., Karz, H.E., and Dirk, C.W., JOSA, B 6, 1339 (1989).Google Scholar
2. Nahata, A., Shan, J., Yardley, J.T., and Wu, C., JOSA B, to be published.Google Scholar
3. Nahata, A., Shan, J., Yardley, J.T., and Wu, C., JOSA B 10, 1554 (1993).Google Scholar
4. See for example Lytel, R., Lipscomb, G.F., Binkley, E.S., Kenny, J.T., and Ticknor, A.J., Materials for Nonlinear Optics: Chemical Perspectives (ACS, 1991), Chapter 6, p. 106.Google Scholar
5. See for example Lampsch, H.L., Yang, J., Wong, G.K., and Torkelson, J.M., Polymer Comm., 30, 40 (1989);Google Scholar
Singer, K.D. and King, L.A., J. Appl. Phys., 70, 3251 (1991);Google Scholar
Man, H.-T. and Yoon, H. N., Adv. Mater. 4, 159 (1992);Google Scholar
Lindsay, G.A., Henry, R.A., Hoover, J.M., Knoesen, A., and Mortazavi, M.A., Macromolecules, 25, 4884 (1992).Google Scholar
6. Polyvinylphenol kindly provided by Hoechst Celanese Inc.Google Scholar
7. Osuch, C.E., Brahim, K., Hopf, F.R., McFarland, M.J., Mooring, A., and Wu, C., Proc. SPIE, 631, 68 (1986).Google Scholar
8. Karshak, V.V., Vinogradova, S.V., and Vygodskii, Y.S., J. Macromol. Sci. Rev. Macromol. Chem., C11, 45 (1974).Google Scholar
9. Morgan, P. W., Macromolecules, 4, 536, (1971).Google Scholar
10. Jonker, S.A. and Warman, J.W., ACS Polymer Reprints 32–3, 142 (1991).Google Scholar
11. Nahata, A., Wu, C., and Yardley, J.T., IEEE Trans, on Instrumentation and Measurement, 41, 128 (1992).CrossRefGoogle Scholar
12. The number M =2.5 indicates that the polymer contained equal amounts of diacid where M=2 andm=3.Google Scholar