AFM, TEM and nanoindentation characterizations of plastic deformation in metallic multilayers

Published online by Cambridge University Press:  17 November 2003

Get access

Abstract

This communication presents experimental observations of plastic deformation in submicronic metallic multilayers. As the length scale decreases down to the nanometer range, we evidence a major change in deformation mechanisms, plasticity becoming less localized as in traditional slip bands of dislocations. AFM and nanoindentation techniques are used in conjonction with more standard techniques to characterize plastic deformation.

Information

Type
Research Article
Copyright
© La Revue de Métallurgie, 2003

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable