Hostname: page-component-586b7cd67f-l7hp2 Total loading time: 0 Render date: 2024-11-25T00:54:52.010Z Has data issue: false hasContentIssue false

(100) Oriented Sputter-deposited Pt Thin Films on MgO/Fe Composite Bilayers using SiO2/Si substrates With Addition of O2 During Pt Sputtering

Published online by Cambridge University Press:  01 February 2011

Shigeki Nakagawa
Affiliation:
nakano.h.aa@m.titech.ac.jp, Tokyo Institute of Technology, Physical Electronics, Tokyo, Japan
Hiroshi Nakano
Affiliation:
murashima.yuji@jp.panasonic.com, Panasonic Electronic Devices Co., Ltd, Osaka, Japan
Yuji Murashima
Affiliation:
komaki.kazuki@jp.panasonic.com, Panasonic Electronic Devices Co., Ltd, Osaka, Japan
Kazuki Komaki
Affiliation:
nakagawa@pe.titech.ac.jp, Tokyo Institute of Technology, Physical Electronics, Tokyo, Japan
Tatsuro Matsumoto
Affiliation:
matsumoto.t.ae@m.titech.ac.jp, Tokyo Institute of Technology, Physical Electronics, Tokyo, Japan
ChongE Wang
Affiliation:
wang.c.ae@m.titech.ac.jp, Tokyo Institute of Technology, Physical Electronics, Tokyo, Japan
Get access

Abstract

Perovskite type oxide thin films have attracted a lot of attention, because they are essential materials which will be used for various electric devices such as ferroelectric random access memory (FeRAM) and tunable filter devices. When the materials are used for such capacitive devices, bottom electrode layers for oxide films are very important, since they significantly affect the crystallinity of the oxide films. Platinum (Pt) is one of the well known bottom electrode materials used for the oxide thin films. Pt provides also better nucleation sites for such perovskite materials due to small lattice misfit. Since dielectric properties of ferroelectric films are originated from the displacement of ions in a crystal along the c-axis direction, c-axis oriented ferroelectric thin films are required to attain better dielectric properties. (100) oriented Pt layers are required to attain c-axis oriented perovskite type ferroelectric films. In our previous report, we succeeded in preparing (100)-oriented Pt thin films with thickness of 20 nm on SiO2/Si substrate at substrate temperature Ts above 400 °C using MgO (100) buffer layers which deposited on Fe (100) seed layers. However, the growth of Pt(111) texture appeared when the thickness was increased from 20 nm to 100 nm, since (100) texture has relatively higher surface energy than (111) closely packed texture for Pt surface. It suggested that surface energy of the films changed during the deposition. In order to keep the surface energy, addition of O2 gas was performed during Pt deposition. Pt thin films with (100) preferred orientation with thickness above 100 nm were deposited on the (100) oriented MgO layer prepared on very thin seed Fe layers deposited on SiO2/Si substrates at Ts of 500 °C by facing-targets sputtering. It was also succeeded to attain (100) oriented perovskite oxide layer when they were deposited on the Pt(100)/Mg(100)/Fe/SiO2/Si underlayer.

Type
Research Article
Copyright
Copyright © Materials Research Society 2010

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

[1] Moazzami, R.: Semicond. Sci. Technol. 10 (1995) 375.Google Scholar
[2] Kim, K.-B., Yun, T.-S., Kim, R.-Y., Kim, H.-S., Kim, H.-G., and Lee, J.-C.: Microwave Opt. Technol. Lett. 45 (2005) 15.Google Scholar
[3] Ahn, K. H. and Baik, S.: Mater. Res. Soc. 17 (2002) 2334.Google Scholar
[4] McIntyre, P. C., Maggiore, C. J., and Nastasi, M.: Acta. Mater. 45 (1997) 869.Google Scholar
[5] McIntyre, P. C., Maggiore, C. J., and Nastasi, M.: Acta. Mater. 45 (1997) 879.Google Scholar
[6] Matsumoto, T, Tamai, K, Murashima, Y, Komaki, K and Nakagawa, S: Jpn. J. Appl. Phys. 47 (2008) 7565.Google Scholar
[7] Lotgering, F. K.: J. Inorg. Nucl. Chem. 9 (1959) 113.Google Scholar
[8] Li, X., Sakurai, A., Shiratsuyu, K., Tanaka, K., and Sakabe, Y.: Proc. of ISAF 2000 12th IEEE Int. Symposium on the Applications of Ferroelectrics 2 (2000) 909.Google Scholar
[9] Shi, J., Kojima, D., and Hashimoto, M.: J. Appl. Phys. 88 (2000) 1679.Google Scholar
[10] Chen, T., Li, X. M., and Zhang, S.: Solid State Commun. 131 (2004) 523.Google Scholar
[11] Chen, T. L., Li, X. M., Zheng, S., and Zhang, X.: Appl. Phys. A 80 (2005) 73.Google Scholar
[12] Chen, T. L., Li, X. M., and Zhang, X.: Appl. Phys. A 79 (2004) 1857.Google Scholar
[13] Masuda, A., Yamanaka, Y., Tazoe, M., and Yonezawa, Y.: Jpn. J. Appl. Phys. 34 (1995) 5154.Google Scholar
[14] Matsumoto, T, Tamai, K, Murashima, Y, Komaki, K and Nakagawa, S 2009 ICMAT: Int. Conf. on Materials for Advanced Technologies (Singapore).Google Scholar