Dislocations Microstructures and Disorientation of Cubic Planes in Samples of a Superalloy Submitted to Bending Tests

Published online by Cambridge University Press:  26 February 2011

J.Y. Buffiere
Affiliation:
Laboratoire de Thermodynamique et Physico-Chimie Métallurgiques, E.N.S.E.E.G, BP.75, 38402 Saint Martin d'Hères, France
M. Ignat
Affiliation:
Laboratoire de Thermodynamique et Physico-Chimie Métallurgiques, E.N.S.E.E.G, BP.75, 38402 Saint Martin d'Hères, France
P. Bastie
Affiliation:
Laboratoire de Spectrométrie Physique Université Joseph Fourier Grenoble, Saint Martin d'Hères, France
Get access

Abstract

Single crystal samples of a nickel base superalloy have been deformed by cyclic bending tests. At the higher temperatures of our experiments, an evolution of the apparent modulus as the advancement of disorientation of cubic planes has been detected.

The dislocation microstructures show that the development of dislocation networks is more advanced in the compressive zones than in the tensile ones.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 1991

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

1- Ezz, S.S., Pope, D.P. and Paidar, V., the tension/compression flow stress asymmetry in Ni3(Al,Nb) single crystals. Acta Metall., Vol. 30, p.921926 (1982).Google Scholar
2- Umakoshi, Y., Pope, D.P. and Vitek, , The asymmetry of the flow stress in Ni3 (Al, Ta) single crystals Acta Metall., Vol. 32, p.449 456 (1984).Google Scholar
3- Miner, R.V., Gabb, T.P., Gayda, J. and Hemker, K.J., Orientation and temperature dependence of some mechanical properties of the single, crystal Nicckel-base superalloy René N.4: Part III. Tension compression Anisotropy, Met. Trans. A Volume 17A, March (1986).Google Scholar
4- Shah, D.M. and Duhl, D.N., the effect of orientation, temperature and Ɣ' prime size on the yeld strength of a single crystal nickel base superalloy. Proc. “Superalloys 84” Seven Springs (USA) p. 105-114 (1984).Google Scholar
5- Heredia, F.E. and Pope, D.P., The Tension/compression flow asymmetry in a high volume fraction nickel base alloy. Acta Metall., Vol.34 (2) p.279 285 (1986).Google Scholar
6- Milligan, W.W. and Autolovitch, S.D., On the mechanism of cross slip in Ni3 Al, Met. Trans. A, Vol. 20A, p.2811.Dec. (1989)CrossRefGoogle Scholar
7- Caron, P., Khan, T. “Improvment of creep strength in a Ni base single crystal by heat treatment Mat. Sci. Eng., 61, p. 173 (1983).Google Scholar
8- Timoshenko, S.P., Gere, J.M., Strengths of Materials Van Nostrand Rheinhold Company Editor (1972).Google Scholar
9- Bastie, P., Lajzerowicz, J., La diffractometrieƔ, une technique pour éudier la mosaïcité des superalliages. Proceedings of the National Symposium on Single Crystalline Superalloys Feb. (1986).Google Scholar