Exploiting Silicon Porosity Gradients for Superior Antireflective Films

Published online by Cambridge University Press:  11 February 2011

Christopher C. Striemer
Affiliation:
Department of Electrical and Computer Engineering, University of Rochester, Rochester, NY 14627, U.S.A.
Philippe M. Fauchet
Affiliation:
Department of Electrical and Computer Engineering, University of Rochester, Rochester, NY 14627, U.S.A.
Get access

Abstract

An electrochemical etching technique has been developed that provides continuous control over the porosity of a porous silicon (PSi) layer as a function of etching depth. Thin films with engineered porosity gradients, and thus a controllable refractive index gradient, have been used to demonstrate broadband antireflection (AR) properties on silicon wafers and solar cell substrates. This low broadband reflectivity is a direct result of the formation of a refractive index gradient at the substrate surface, where the transition between air and silicon occurs continuously throughout the thickness of a PSi film. These graded index films are formed by applying a continuously changing current function to the electrochemical cell during the PSi etch. The application of these films as solar cell AR coatings is of particular interest, where their broadband nature is a critical advantage. For this application, graded index PSi films must not only offer superior AR properties, but must also prove minimally disruptive to the electrical properties of the underlying solar cell. This requirement limits the total thickness of these films to approximately 120 nm, creating several challenges for this process. However, the simplicity and highly reproducible nature of this technique, in combination with its short duration (less than 10 seconds), make it a strong alternative to current vacuum deposited AR coating technology.

Type
Research Article
Copyright
Copyright © Materials Research Society 2003

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

Krotkus, A., Grigoras, K., Pacebutas, V., Barsony, I., Vazsonyi, E., Fried, M., Szlufcik, J., Nijs, J., and Levy-Clement, C., Sol. Energy Mat. Sol. Cells 45, 267 (1997).Google Scholar
[2] Stalmans, L., Poortmans, J., Bender, H., Caymax, M., Said, K., Vazsonyi, E., Nijs, J., and Mertens, R., Prog. Photovolt. Res. Appl. 6, 233 (1998).Google Scholar
[3] Theiss, W., Surface Science Reports 29, 91 (1997).Google Scholar
[4] Thonissen, M., Berber, M.G., Billat, S., Arens-Fischer, R., Kruger, M., Luth, H., Theiss, W., Hillbrich, S., Grosse, P., Lerondel, G., Frotscher, U., Thin Solid Films 297, 92 (1997).Google Scholar
[5] Zangooie, S., Jansson, R., and Arwin, H., Mat. Res. Soc. Proc. 557, 195 (1999).Google Scholar
[6] Berger, M.G., Arens-Fischer, R., Thonisson, M., Kruger, M., Billat, S., Luth, H., Hilbrich, S., Theiss, W., and Grosse, P., Thin Solid Films 297, 237 (1997).Google Scholar
[7] Uehara, S., Kurose, K., and Matsubara, T., Phys. Stat. Sol. (a) 182, 461 (2000).Google Scholar
[8] Striemer, C.C. and Fauchet, P.M., Appl. Phys. Lett. 81, 2980 (2002).Google Scholar
[9] Hiller, J., Mendelsohn, J.D., and Rubner, M.F., Nature Mat. 1, 59 (2002).Google Scholar
[10] Chan, S. and Fauchet, P.M., Appl. Phys. Lett., 75, 274 (1999).Google Scholar
[11] Hanoka, J.I., Sol. Energy Mat. Sol. Cells 65, 231 (2001).Google Scholar
[12] Jacobsson, R., in Progress in Optics, vol. 5, edited by Wolf, E. (John Wiley & Sons, New York, 1965) pp. 249.Google Scholar
[13] Hecht, E. and Zajac, A., Optics (Addison-Wesley, London, 1974) pp. 311.Google Scholar
[14] Handbook of Optical Constants of Solids, edited by Palik, E.D. (Harcourt Brace Jovanovich, New York, 1985) pp. 561.Google Scholar
[15] Brumhead, D., Canham, L.T., Seekings, D.M., and Tufton, P.J., Electrochimica Acta 38, 191 (1993).Google Scholar