Hardness of Thin Films Determined Based on Nanoindentation Load and Contact Stiffness

Published online by Cambridge University Press:  10 February 2011

D. S. Stone
Affiliation:
Materials Science and Engineering, University of Wisconsin-Madison
M. F. Tambwe
Affiliation:
Materials Science and Engineering, University of Wisconsin-Madison
H. Kung
Affiliation:
Division of Materials Science and Technology, Los Alamos National Laboratory
M. Nastasi
Affiliation:
Division of Materials Science and Technology, Los Alamos National Laboratory
Get access

Abstract

A model for the elastic contact between an indenter and a layered half-space allows the projected contact area to be estimated based on measured contact stiffness. In this way, the model allows the hardness to be determined indirectly based solely on load and contact stiffness rather than load and contact area. We apply the approach to Cu, Nb, and Cu/Nb multilayer thin films on Si.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 1998

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

[1] Stone, D.S.. Accepted by J. Mater. Res. (1998)Google Scholar
[2] Yoder, K.B., Stone, D.S., Hoffinan, R.A., and Lin, J.C.. Accepted by J. Mater. Res (1998).Google Scholar
[3] Loubet, J.L., Georges, J.M., and Meille, G.. ASTM STP 889, P.J. Blau and B.R. Lawn, Eds. (1986) pp. 7289 Google Scholar
[4] Doemer, M.F. and Nix, W.D., J. Mater. Res. 1(4), 601 (1986)Google Scholar
[5] Stone, D. S., Yoder, K. B., and Sproul, W. D., J. Vac. Sci. Tech. A 9(4) 25432547 (1991).Google Scholar
[6] Tambwe, M.F., Stone, D.S., Hirvonen, J.-P., Suni, I., and Hannula, S.-P.. Scripta Mater., 37, 14211427 (1997)Google Scholar
[7] King, R.B., Int. J. Solids Structures, 23(12), 16571664 (1987)Google Scholar
[8] Cheng, Y.-T. and Cheng, C.-M.. Phil. Mag. Let. 77(1), 3947 (1998)Google Scholar
[9] Bolshakov, A. and Pharr, G.M., Mat. Res. Symp. Proc., Vol.436. (1996), pp.146151.Google Scholar
[10] Joslin, D.L. and Oliver, W.C.. J Mater.Res. 5, 123126 (1990)Google Scholar
[11] Simmons, G. and Wang, H.. Single Crystal Elastic Constants and Calculated Aggregate Properties: A Handbook, 2nd Ed. (MIT Press, Cambridge MA, 1971) 262.Google Scholar
[12] Bhushan, B. and Gupta, B.K.. Handbook of Tribology (McGraw- Hill, New York, NY, 1991) 15.42.Google Scholar
[13] Stone, D.S. and Yoder, K.B.. J. Mater. Res., 9(10) 25242533 (1994).Google Scholar