Hostname: page-component-586b7cd67f-gb8f7 Total loading time: 0 Render date: 2024-11-24T17:34:26.530Z Has data issue: false hasContentIssue false

High Quality Sn-Doped In2O3 Films Grown by Pulsed Laser Deposition for Organic Light-Emitting Diodes

Published online by Cambridge University Press:  15 February 2011

Heungsoo Kim
Affiliation:
Code 6372 1 and Code 5615 2 Naval Research Laboratory, 4555 Overlook Avenue, SW, Washington DC, 20375, U.S.A.
James S. Horwitz
Affiliation:
Code 6372 1 and Code 5615 2 Naval Research Laboratory, 4555 Overlook Avenue, SW, Washington DC, 20375, U.S.A.
Woo Hong Kim
Affiliation:
Code 6372 1 and Code 5615 2 Naval Research Laboratory, 4555 Overlook Avenue, SW, Washington DC, 20375, U.S.A.
Zakya H. Kafafi
Affiliation:
Code 6372 1 and Code 5615 2 Naval Research Laboratory, 4555 Overlook Avenue, SW, Washington DC, 20375, U.S.A.
Douglas B. Chrisey
Affiliation:
Code 6372 1 and Code 5615 2 Naval Research Laboratory, 4555 Overlook Avenue, SW, Washington DC, 20375, U.S.A.
Get access

Abstract

High quality Sn-doped In2O3 (ITO) thin films have been grown by pulsed laser deposition (PLD) on glass, flexible polyethylene terephthalate (PET) and single crystal yttria stabilized zirconia (YSZ) substrates for use in organic light emitting diodes (OLEDs). Critical electrode issues for the OLED are related to the optical transparency, electrical resistivity, work function and surface roughness of the ITO film. Our research has focused on improving the properties of the ITO film to increase the efficiency of the OLED. Films were deposited using a KrF excimer laser (248nm, 30 ns FWHM) at fluences of 2 J/cm2 at substrate temperatures ranging from 1 to 100 mTorr. For ITO films (∼ 100 nm thick) deposited at the optimized conditions, a resistivity of 4.1 × 10-4 Ω-cm, 2.2 × 10-4 Ω-cm, 1.8 × 10-4 Ω-cm was observed on PET, glass and YSZ, respectively. The average film transmission in the visible range (400 - 700 nm) was about 90 % and the film surface roughness was about 0.5 nm for the film grown on glass. The Hall mobility and carrier density for ITO films (300 nm thickness) were observed to be in the range of 28 - 34 cm2/V-s and 1.0 - 1.2 × 1021 cm-3, respectively. We have used the ITO films, deposited by PLD on glass, plastic and single crystal YSZ substrates, as an anode contact in OLEDs. The OLED device performance based on PLD ITO anodes is compared with that of the device fabricated on the commercial ITO anode.

Type
Research Article
Copyright
Copyright © Materials Research Society 2003

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

1. Hartnagel, H. L., Dawar, A. L., Jain, A. K. and Jagadish, C., “Semiconducting Transparent Thin Films” (Institute of Physics Publishing, 1995).Google Scholar
2. Minami, T., J. Vac. Sci. Technol. A 17, 1765 (1999)Google Scholar
3. Kawazoe, H., Yanagi, H., Ueda, K., and Hosono, H., MRS Bull. 25, 28 (2000)Google Scholar
4. Kim, H., Gilmore, C. M., Horwitz, J. S., Piqué, A., Murata, H., Kushto, G. P., Schlaf, R., Kafafi, Z. H. and Chrisey, D. B., Appl. Phys. Lett. 76, 259 (2000)Google Scholar
5. Chopra, K. L., S. Major and Pandya, D. K., Thin Solid Films 102, 1 (1983)Google Scholar
6. Manifacier, J. C., Thin Solid Films 90, 297 (1982)Google Scholar
7. Vossen, J. L., Phys. Thin Films 9, 1 (1977)Google Scholar
8. Kim, H., Horwitz, J. S., Kim, W. H., Kafafi, Z. H., and Chrisey, D. B.: J. Appl. Phys. 91, 5371 (2002)Google Scholar
9. Kim, H., Piqué, A., Horwitz, J. S., Mattoussi, H., Murata, H., Kafafi, Z. H. and Chrisey, D. B., Appl. Phys. Lett. 74, 3444 (1999)Google Scholar
10. Kim, H., Gilmore, C. M., Piqué, A., Horwitz, J. S., Mattoussi, H., Murata, H., Kafafi, Z. H. and Chrisey, D. B., J. Appl. Phys. 86, 6451 (1999)Google Scholar
11. Chrisey, D. B. and Hubler, G. K., Pulsed Laser Deposition of Thin Films, (Wiley, New York, 1994).Google Scholar
12. Avaritsiotis, J. N. and Howson, R. P., Thin Solid Films 77, 351 (1981)Google Scholar
13. Schroder, D. K., Semiconductor Material and Device Characterization, (John Wiley & Sons, New York, 1990).Google Scholar
14. Kim, W. H., Makinen, A. J., Nikolov, N., Shashihhar, R., Kim, H., and Kafafi, Z. H., Appl. Phys. Lett. 80, 3844 (2002)Google Scholar
15. Murata, H., Merritt, C. D. and Kafafi, Z. H., IEEE J. Sel. Topics in Quant. Elec. 4(1), 119, (1998).Google Scholar
16. Daly, G. M., H. Murata, Merritt, C. M., Kafafi, Z. H., Inada, H., and Shirota, Y., MRS Proc. 488, 33 (1998)Google Scholar
17.JCPDS Card No. 06–0416.Google Scholar
18.JCPDS Card No. 30–1468.Google Scholar