Nanoindentation as a Tool for Formation of Thin Film-Based Barrier Structures

Published online by Cambridge University Press:  01 February 2011

H. Khlyap
Affiliation:
University of Technology, E.-Schroedinger str. 56, D-67663 Kaiserslautern, Germany, and State Pedagogical University, 24 Franko str., 82100 Drohobych, Ukraine
P. Sydorchuk
Affiliation:
State Pedagogical University, 24 Franko str., 82100 Drohobych, Ukraine
Get access

Abstract

A2B6 semiconductors and their solid solutions (ZnSe, ZnTe, CdTe, ZnCdHgTe) are matter of choice for near- and far-infrared optoelectronics. The importance of maximally reduced degree of defectness for these materials is not subjected to discussion. However, preparation of high quality barrier structures based on these compounds by means of MBE, laser technology or liquid phase technique is not always successful due to lattice parameters mismatch. At the same time, good selection of a proper buffer layer may also pose some unavoidable problems. From this point of view the nanoindentation as a tool of defect engineering can be effective for fabrication of surface barrier structures. The first experimental results and numerical simulation of experimental data obtained under investigation of nanoindentation effect on electric characteristics (in particular, current – voltage (I-V) and capacitance – voltage (C-V)) of ZnCdHgTe thin films and ZnCdHgTe/Cd(Zn)Te heterostructures at the room temperature are presented.

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

[1] Khlyap, H., Sydorchuk, P., Polit, J., Oszwaldowski, M.. MRS Proceedings 785 (2004) D.10.Google Scholar
[2] Guergouri, K., Brihi, N., Triboulet, R., J. Cryst. Growth 49, 709 (2000).Google Scholar
[3] Sydorchuk, P., Khlyap, G., Andrukhiv, A., Cryst. Res. Tech. 36, 361 (2001).Google Scholar
[4] Hernandez, E., Cryst. Res. Tech. 33, 285 (1998).Google Scholar