Hostname: page-component-586b7cd67f-dsjbd Total loading time: 0 Render date: 2024-11-25T20:55:19.395Z Has data issue: false hasContentIssue false

Water Uptake and Conduction in Strontium Ytterbium Cerate

Published online by Cambridge University Press:  16 February 2011

G. W. Coffey
Affiliation:
Washington State University at Tri-Cities, Richland, Washington 99352, USA
L. R. Pederson
Affiliation:
Pacific Northwest Laboratory, P.O. Box 999, Richland, Washington 99352, USA
W. J. Weber
Affiliation:
Pacific Northwest Laboratory, P.O. Box 999, Richland, Washington 99352, USA
Get access

Abstract

Water uptake and conduction have been studied in SrYb0.05Ce0.95O3-δ, a composition known to conduct protons, oxygen ions, and electrons, depending on temperature and environment. Water uptake kinetics evaluated by thermogravimetry occurred in two distinct stages: a rapid, initial weight gain (0.39±0.09 eV, attributed to grain boundary and near surface hydration) followed by a much slower uptake (2.8±0.4 eV, attributed to hydration of the bulk grains). From cyclic voltammetry and mass spectrometry measurements for a cell exposed to asymmetric conditions, currents and activation energies for electronic, oxygen ion, and proton conduction were determined. The activation energy for electronic conduction, 0.90±0.09 eV, is believed to be artificially high due to the increase in electron carrier concentration with increased temperature. The activation energy for oxygen ion conduction (0.97±0.10 eV) agrees well with other oxygen conductors. Proton conduction appeared to follow two different mechanisms: a low temperature process characterized by an activation energy of 0.42±0.04 eV, and a high temperature process, characterized by an activation energy of 1.38±0.13 eV. A possible explanation is that proton conduction at low temperatures is dominated by grain boundaries and is dominated by bulk conduction at higher temperatures.

Type
Research Article
Copyright
Copyright © Materials Research Society 1995

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

[1] Norby, T., Solid State Ionics 40/41, 857 (1990).Google Scholar
[2] Bonanos, N., Solid State Ionics 53-56, 967 (1992).Google Scholar
[3] Iwahara, H., Solid State Ionics 28-30, 573 (1988).Google Scholar
[4] Iwahara, H., Yajima, T., Hibino, T., and Ushida, H., J. Electrochem. Soc. 140 [6] 1687 (1993).Google Scholar
[5] Hamakawa, S., Hibino, T., and Iwahara, H., J. Electrochem. Soc. 141 [7] 1720 (1994).Google Scholar
[6] Yajima, T., Iwahara, H., and Uchida, H., Solid State Ionics 47, 117 (1991).Google Scholar
[7] Bonanos, N., Ellis, B., and Mahmood, M. N., Solid State Ionics 44, 305 (1991).Google Scholar
[8] Scherban, T. and Nowick, A. S., Solid State Ionics 35, 189 (1989).Google Scholar
[9] Cook, R. L. and Sammells, A. F., Solid State Ionics 45, 311 (1991).Google Scholar
[10] Chick, L. A., Pederson, L. R., Maupin, G. D., Bates, J. L., Thomas, L. E., and Exarhos, G. J., Materials Letters 10, 6 (1990).Google Scholar
[11] Armstrong, T. R., Bates, J. L., Coffey, G. W., Kingsley, J. J., Pederson, L. R., Stevenson, J. W., Weber, W. J., and Youngblood, G. E., Proc. 8th Annual Conf. on Fossil Energy Materials, CONF-9405143, Oak Ridge National Laboratory, Oak Ridge, Tennessee (1994) p. 89.Google Scholar
[12] Iwahara, H., Solid State Ionics 52, 99 (1992).Google Scholar
[13] Iwahara, H., Yajima, T., Hibino, T., and Ushida, H., J. Electrochem. Soc. 140 [6] 1687 (1993).Google Scholar
[14] Tuller, H. L., in Ceramic Materials for Electronics, ed. Buchanon, R. C., Marcel Dekker, New York (1986) p. 425.Google Scholar
[15] Kreuer, K. D., Schonherr, E., and Maier, J., Proc. 14th Int. Symp. Materials Science, eds. Poulson, F. W., Bentzen, J. J., Jacobsen, T., Skou, E., and Ostergard, M. L. J., Riso National Laboratory, Roskilde, Denmark (1993) p. 297.Google Scholar